Avoid glass lined reaction tank damage precautions

Shandong Tanglian always adhere to the "quality-oriented",with high quality products and perfect after-sales service to win the trust of customers and high praise, the products are sold at home and abroad. The following are the precautions to avoid damage to the glass lined reactor:

In the process of installing and using glass-lined reactor, there are often improper operations leading to equipment damage, especially the fragile glass-lined layer on the inner surface of the reactor. After the equipment is damaged, it has to be repaired, which is a waste of money and delayed work. So let's talk about what behavior in the operation is easy to cause damage to the reactor equipment, and then we should avoid these behaviors in the use:

  1. When installing glass-lined reactor cover and stirring, we should pay attention to avoiding hard touching;

  2. Installation of kettle cover, feed port, discharge port should be in accordance with the provisions of the symmetrical tightening of bolts;

  3. Use wooden ladder and rubber shoes for checking under kettle;

  4. To regularly check the integrity of the stirring lock mother, to prevent the lock mother damage reducer reversal to make the stirring off;

  5. When installing the flange and switching manhole cover, nothing should be dropped down;

  6. When welding on glass-lined kettle or kettle, the porcelain surface should be protected, and the welding slag should never fall on the porcelain surface;

  7. Enameled kettle in the uncooled, can not add material, to prevent the porcelain surface cold burst porcelain;

  8. Jacket through the steam heating, according to regulations, can not be heated too vigorously;

  9. Steam heating or steam valve leakage, the water in the jacket should be released. Otherwise, it may lead to a large temperature difference between the upper and lower kettle, so that the residual stress is greater enamel kettle temperature low parts of the stress exerted and a large area of bursting porcelain;

  10. To choose corrosion-resistant mat to prevent material leakage, corrosion enamel;

  11. kettle crystallization, absolutely can not use iron bar barrel, hammer smash; add material can not be added along the kettle wall.

  In short, we should regularly check the glass-lined reactor, timely detection of equipment such as bursting other problems, make a record and then repair. In addition is in the kettle charging, if found glass lining debris should also be timely parking, shall not continue to work, find out the reasons for damage to the equipment, and then take timely remedial measures.

Need to know more about the content of the reactor and other pressure vessels, please continue to pay attention to us.

文章5.jpg

Contact Us

Tel: +86 18678188295

E-mail: service@chinareactor.com

Add: Hongshan Town Industrial Park, Chongzheng Road, Zichuan District, Zibo City, Shandong Province