What is the thickness of the glass layer of the glass-lined reactor?

Many companies believe that is not related to the quality and service life of the glass lined equipment. In fact, it is not right. The workers must strictly follow the thickness standard during the manufacturing process.

Is the thickness of the glass lined equipment layer used in different industries different? It is not the same. Because the use of different industries is different, we have corresponding standards for the use of different industries.

If the customer has additional requirements for the product, we can adjust the thickness of the glass layer according to the customer's needs.

The thickness of the glass lined equipment layer is 0.8 to 2.0 mm. When the nominal volume is greater than or equal to 10000L, the upper limit of the thickness may be allowed to 2.2mm; when the nominal volume is greater than or equal to 20,000L, the upper limit of the thickness may be allowed to be 2.4mm. The thickness of the glass lined equipment layer of the finished mechanical seal section of the glass-lined equipment can be allowed to be 0.6 mm. The thickness of the bismuth glass layer should be as uniform as possible, and the thickness of the glass lined equipmen layer should be thin at the convex portion, and the thick and thin regions should be smoothly transitioned.IMG_0949.JPG

 